Improvement of Coercivity and Curie Temperature of Sintered Nd-Fe-B Permanent Magnets by Addition of Cu and Ni
MakaleYalnız künye
Özet
Sintered Nd-Fe-B magnets are some of the strongest magnetic materials showing magnetic properties. Blending addition is frequently performed in order to improve the magnetic properties of these materials. In this work, high-melting point Ni and low-melting point Cu were added to Nd15Fe77B8 ingot by blending. As a result of structural analysis, it was observed that 0.2 wt% Cu + Ni addition improved the structure of the material; on the other hand, excessive addition resulted in porosity. It was also observed that 0.2 wt% addition improved the magnetic properties, and Curie temperature increased with increasing addition ratio.
Anahtar Kelimeler
RDL Kalıcı Bağlantı (PID)
https://rdlopen.rawdatalibrary.net/r/gumushane/11883Resmi atıflarda kullanılan kalıcı adresTam Kayıt
| Alan | Değer | Dil |
|---|---|---|
| dc.contributor.author | Başoğlu, M. | |
| dc.contributor.author | Yanmaz, E. | |
| dc.date.accessioned | 2026-10-22T10:19:27.312699641Z | |
| dc.date.available | 2026-10-22T10:19:27.312699641Z | |
| dc.date.issued | 2014 | |
| dc.description.abstract | Sintered Nd-Fe-B magnets are some of the strongest magnetic materials showing magnetic properties. Blending addition is frequently performed in order to improve the magnetic properties of these materials. In this work, high-melting point Ni and low-melting point Cu were added to Nd15Fe77B8 ingot by blending. As a result of structural analysis, it was observed that 0.2 wt% Cu + Ni addition improved the structure of the material; on the other hand, excessive addition resulted in porosity. It was also observed that 0.2 wt% addition improved the magnetic properties, and Curie temperature increased with increasing addition ratio. | |
| dc.identifier.doi | 10.1007/s10948-014-2582-4 | |
| dc.identifier.eissn | 1557-1947 | |
| dc.identifier.endpage | 2298 | |
| dc.identifier.issn | 1557-1939 | |
| dc.identifier.issue | 10 | |
| dc.identifier.scopus | 2-s2.0-84912050341 | |
| dc.identifier.startpage | 2295 | |
| dc.identifier.uri | https://rdlopen.rawdatalibrary.net/r/gumushane/11883 | |
| dc.identifier.volume | 27 | |
| dc.identifier.wos | WOS:000343162400017 | |
| dc.language.iso | en | |
| dc.publisher | Springer Science and Business Media, LLC | |
| dc.relation.ispartof | Journal of Superconductivity and Novel Magnetism | |
| dc.rights | info:eu-repo/semantics/closedAccess | |
| dc.subject | Blending addition | |
| dc.subject | Copper | |
| dc.subject | Nd-Fe-B magnets | |
| dc.subject | Nickel | |
| dc.subject | Sintered magnets | |
| dc.subject.classification | Physics, Applied | |
| dc.subject.classification | Physics, Condensed Matter | |
| dc.subject.classification | Physics | |
| dc.subject.other | Blending | |
| dc.subject.other | Copper | |
| dc.subject.other | Curie temperature | |
| dc.subject.other | Iron alloys | |
| dc.subject.other | Magnetic materials | |
| dc.subject.other | Magnetic properties | |
| dc.subject.other | Magnetism | |
| dc.subject.other | Magnets | |
| dc.subject.other | Materials properties | |
| dc.subject.other | Melting point | |
| dc.subject.other | Nickel | |
| dc.subject.other | Sintering | |
| dc.subject.other | High melting point | |
| dc.subject.other | Low melting point | |
| dc.subject.other | Nd fe b permanent magnets | |
| dc.subject.other | Nd-Fe-B magnets | |
| dc.subject.other | Ni additions | |
| dc.subject.other | Sintered magnets | |
| dc.subject.other | Sintered NdFeB magnet | |
| dc.subject.other | Neodymium alloys | |
| dc.title | Improvement of Coercivity and Curie Temperature of Sintered Nd-Fe-B Permanent Magnets by Addition of Cu and Ni | |
| dc.type | Article | |
| dspace.entity.type | Publication | |
| rdl.citation.openalex | 1 | |
| rdl.citation.scopus | 1 | |
| rdl.citation.wos | 1 | |
| rdl.oa.status | closed | |
| rdl.source.index | SCOPUS | |
| rdl.source.index | WOS | |
| rdl.wos.index | Science Citation Index Expanded (SCI-EXPANDED) |